Abstract:For preventing the edge cracking produced in hot-rolling grain-oriented silicon steel,some measures are adopted: controlling ,oxygen concentrate and hold time in atmosphere when slab heating above 1200℃,adjusting reduction and rolling temperature of roughing mill,carrying out width reduction and brink heating,changing deformation energy of material and inhibiting brink fish scale -type defect. Results show that these are effective for decreasing the formation of edge cracking.
卢凤喜, 黄 璞. 川崎取向硅钢热轧边裂及其防止方法[J]. 中国冶金, 2006, 16(7): 1-1.
Lu Feng-xi HuangPu. Edge Cracking of Hot-rolling Grain-oriented Silicon Steel and Its preventive method in KAWASAKI STEEL. China Metallurgy, 2006, 16(7): 1-1.