Abstract:The experiences in handling long term blow-down of 2300m3 BF in Ling Steel were summarized,including holding temperature after blow-down;adding appropriate clean coke at the beginning of reblowing and more coal to make the blast temperature enough;reducing the basicity of slag to improve the slag liquidity;moderately adjusting the ore batch and burden distribution matrix to ensure the reasonable distribution of the two gas flow;hierarchically plugging the tuyere and reasonably arranging the blast furnace casthouse operation etc. Finally, it took only 24h to make the furnace condition normal after reblowing.
马晓勇,张宝付,戴田军,李亮. 凌钢2300m3高炉长期非计划休风快速恢复炉况[J]. 中国冶金, 2016, 26(7): 39-42.
MA Xiao-yong,ZHANG Bao-fu,DAI Tian-jun,LI Liang. Rapid recovery practice of long term unplanned blowing-down of 2300m3 BF in Lingsteel. China Metallurgy, 2016, 26(7): 39-42.