Cause and Prevention Measures of Skin Blowhole in Welding Gas Cylinder Steel HP295
LI Jipeng1,2,MA Jie1,ZHANG Youyu2
1.Xi’an University of Architecture and Technology, Xi’an 710055,Shanxi, China; 2. Research Institute for Iron and Steels, Jiuquan Iron and Steel Co Ltd, Jiayuguan 735100, Gansu, China
Abstract:The forming reasons of the skin blowhole in welding gas cylinder steel HP295 are analyzed. It is shown that the degree of superheat of molten steel and the deoxidation alloying are main factors for the formation of skin blowhole. Then some measures for preventing and controlling them are proposed.
李积鹏1,2 ,马杰1 ,张有余2. HP295焊瓶钢铸坯皮下气泡的成因分析及防止措施[J]. 中国冶金, 2006, 16(10): 20-20.
LI Jipeng1,2,MA Jie1,ZHANG Youyu2. Cause and Prevention Measures of Skin Blowhole in Welding Gas Cylinder Steel HP295. China Metallurgy, 2006, 16(10): 20-20.